Corundum Mullite Tiles For ITO Target Material Sintering

Product Features

ITO target refers to the Indium Tin Oxide (ITO) film covering PDP, LCD, Organic LED (OLED), and other display panels, which is an essential factor for ensuring purity and transparency.

Reason for Double-Sided Grinding

During the sintering process of ITO target materials, multiple instances of bending and deformation may occur. To ensure the flatness of the target, it is necessary to perform multiple grinding operations, which can increase production costs. To prevent deformation and bending during the sintering process, our high-alumina support plates undergo double-sided grinding, ensuring high flatness and achieving the desired quality for ITO target materials.

Technical Parameters

HR88
Al2O3(%) 88.16
SiO2 (%) 11.5
Fe2O3(%) 0.08
Suggested Working Temperature (˚C) 1650
Flatness Tolerance(mm) 8
Standard Size
1000 x 500 x 35-40T 900 x 450 x 35T
800 x 425 x 35T 700 x 400 x 35T
600 x 400 x 30-35T 500 x 500 x 35T

 