Corundum Mullite Tiles For ITO Target Material Sintering
Product Features
ITO target refers to the Indium Tin Oxide (ITO) film covering PDP, LCD, Organic LED (OLED), and other display panels, which is an essential factor for ensuring purity and transparency.
Reason for Double-Sided Grinding
During the sintering process of ITO target materials, multiple instances of bending and deformation may occur. To ensure the flatness of the target, it is necessary to perform multiple grinding operations, which can increase production costs. To prevent deformation and bending during the sintering process, our high-alumina support plates undergo double-sided grinding, ensuring high flatness and achieving the desired quality for ITO target materials.
Technical Parameters
| HR88 | |
| Al2O3(%) | 88.16 |
| SiO2 (%) | 11.5 |
| Fe2O3(%) | 0.08 |
| Suggested Working Temperature (˚C) | 1650 |
| Flatness Tolerance(mm) | 8 |
| Standard Size | |
| 1000 x 500 x 35-40T | 900 x 450 x 35T |
| 800 x 425 x 35T | 700 x 400 x 35T |
| 600 x 400 x 30-35T | 500 x 500 x 35T |